MS

MS – General Purpose Mild Steel

Mild Steel (MS) is a low-carbon, unalloyed steel widely used across the engineering, manufacturing, construction and fabrication industries. It is characterised by its good ductility, weldability, machinability and formability, making it a versatile and economical material for general engineering applications.

With its relatively low carbon content, mild steel offers good flexibility and can be readily processed through conventional machining, cutting, bending, drilling and welding operations. It provides a practical combination of strength, workability and cost-effectiveness, making it suitable for components that do not require high hardness or specialised heat-treatment properties.

Mild Steel is commonly supplied in the as-rolled condition and is available in various shapes and dimensions to meet different industrial requirements. Its ease of fabrication and adaptability make it one of the most widely used materials in general engineering and manufacturing.

Typical uses are: General Engineering Components, Machine Frames, Shafts, Rollers, Bushes, Pins, Brackets, Structural Supports, Fabricated Assemblies, Mounting Plates, Industrial Machinery Components and General-Purpose Fabrication Parts.

Equivalent Grades – MS

EU
EN
USA
–
Germany
DIN,WNr
Japan
JIS
France
AFNOR
England
BS
Italy
UNI
Spain
UNE
China
GB
Sweden
SS
Poland
PN
Czechia
CSN
Austria
ONORM
Russia
GOST
Inter
ISO
C16E / C15E SAE 1018 / AISI 1018 C16.8 / 1.0453 S17C AF42 080A17 C15 C15E 15# — C15 — C15 15
C15 / C18E

Available Types & Range

Available Types & Range

C 40 steel Supply Form & Size

Form of Supply Size(mm) Length(mm)
Round bar Φ20-Φ650 Standard or As your request
Square bar 25 x 25 – 450 x 450 Standard or As your request
Plate/Sheet Thickness :6 – 300
Width:80-1,250
Standard or As your request
Flat bar/Blcoks Thickness :10 – 300
Width:120-25 – 500
Standard or As your request

Related Specifications

Chemical Composition

Chemical Composition & Technical Specification -C 40

Grade C Si Mn P S
MS 0.15–0.20 – 0.60–0.90 0.040 Max 0.050 Max

Typical Mechanical Properties – As Rolled

Tensile Strength Mpa Approx. 400
Yield Strength Mpa Approx. 220
Elongation on 5.65√S0 % Approx. 25
Hardness HB Approx. 116
Rc Not specified

Forging

Heat to 1150°C–1280°C and hold until the temperature is uniform throughout the section before commencing forging. Avoid excessive soaking at high temperatures to minimise grain growth and surface scaling.

Forging should be completed before the material temperature falls below approximately 900°C. Following completion of forging, the workpiece may be cooled in air.

Heat Treatment

Soft Annealing

Heat to 870°C–910°C, hold until the temperature is uniform throughout the section, and cool slowly in the furnace.

Hardening

MS is not suitable for conventional through-hardening due to its low carbon content. However, it can be surface hardened through carburising followed by an appropriate quenching and tempering treatment.

Normalizing

Heat to 890°C–940°C, hold until the temperature is uniform throughout the section, and cool in still air.

Refining & Hardening
Stress Relieving

Stress relieving may be carried out after heavy machining or welding to reduce residual stresses. Heat to approximately 500°C–650°C, allow the temperature to become uniform throughout the section, and cool slowly or in still air.

Tempering

Tempering is not normally required for MS in its standard as-rolled condition. However, following carburising and case hardening, tempering at approximately 150°C–200°C may be carried out to improve the toughness of the hardened case.

Notes on Heat Treatment

MS is generally supplied in the as-rolled condition and offers good suitability for conventional fabrication and machining operations. Due to its low carbon content, it is not suitable for conventional through-hardening. However, it can be surface hardened through carburising or carbonitriding.

Heating temperatures, holding times and cooling rates depend on the component dimensions, material condition and intended application. Consult a qualified heat-treatment specialist before carrying out heat-treatment operations.

Machining

MS offers good machinability and is suitable for conventional machining operations such as turning, drilling, milling and tapping. Its machinability rating is approximately 78% relative to AISI B1112 free-machining steel.

Suitable cutting tools, feeds and speeds should be selected according to the material condition, component dimensions and machine manufacturer’s recommendations.

Welding

MS has excellent weldability in its as-rolled condition and can be welded using conventional processes, including Manual Metal Arc (MMA), Metal Inert Gas / Metal Active Gas (MIG/MAG) and Tungsten Inert Gas (TIG).

Low-carbon steel welding consumables should be used, with selection based on the component thickness, joint design and service requirements.

Welding Procedurde

Welding should be performed using suitable compatible filler materials and appropriate welding parameters. Preheating is generally not necessary for ordinary sections under normal workshop conditions. For thicker sections, particularly above 50 mm, preheating may be beneficial depending on the welding conditions.

Post Welding

Allow the welded component to cool naturally under controlled conditions. Post-weld stress relieving may be considered after heavy welding or where dimensional stability is important. Any required treatment should be determined according to the component’s application and fabrication requirements.

Note: Welding is not recommended after carburising or carbonitriding, as the hardened surface may be susceptible to cracking.